reintitan
2622
Yes! The galvanic corrosion issue is still out there
Oct 16, 2018,17:27 PM
and is an issue with the materials used rather than a mechanical issue. Tudor should really fix the root cause of both problems.
Comments:
view entire thread
mine works perfect ....... BUT !! ...
By: Bruno.M1 : October 16th, 2018-00:17
mine doesn't have this problem, I believe they did fix it, had probably something to do with the spring that moves the date wheel. A Rolex GMT had a similar problem in the past, they replaced the spring. Not sure which Rolex GMT reference it was now the B...
I have had my BB GMT for several months now... in a nutshell,
By: remarque : October 20th, 2018-15:34
I was one of the very first people to get the Tudor BB GMT in the US (circa June 2018), so I have presumably a very early production watch. I wear my watches for a week or two, then rotate what I wear so that I wear each watch fairly equally and regularly...
Thanks for reporting your experience.
By: reintitan : October 22nd, 2018-17:36
The issue hopefully isn't affecting your watch. Even if it does, you can use the warranty to get it fixed. I'm pretty sure Tudor is either repairing the faulty ones under warranty and/or redesigning/replacing the faulty part(s) so future production watche...